Material / Coating | Temperature (°C) | Temperature (°F) | Time (Seconds) | Pressure | Notes / Tips |
---|---|---|---|---|---|
Sublimation - Polyester Fabrics |
|
|
|
|
|
Polyester Fabric (100% White/Light) for Sublimation | 190 - 200 | 375 - 392 | 45 - 70 | Medium | Mirror image. Pre-press fabric 3-5s. Use protective paper. |
Polyester Blend (min 50% poly, light color) for Sublimation | 185 - 195 | 365 - 385 | 50 - 75 | Medium | Vintage/faded look on lower poly counts. Mirror image. Pre-press. |
Sublimation - Rigid Substrates |
|
|
|
|
|
Ceramic Tiles (Sublimation Coated) | 200 - 205 | 392 - 400 | 240 - 480 (4-8 min) | Medium - Firm | Mirror image. Place tile face up, print face down. Use blowout paper & heat pad. Cool face down. |
Aluminium (Sublimation Coated Sheets & Blanks) | 190 - 200 | 375 - 392 | 50 - 90 | Medium | Remove protective film! Mirror image. Pre-press metal briefly. Cool quickly. |
Hardboard Blanks (Coasters, Keychains for Sublimation) | 190 - 200 | 375 - 392 | 60 - 90 | Medium - Firm | Remove protective film! Mirror image. Pre-press if needed. |
MDF (Sublimation Coated Wood) | 190 - 200 | 375 - 392 | 70 - 120 | Medium | Mirror image. Pre-press. Can warp; cool under weight. |
Mousepads (Polyester Top for Sublimation) | 190 - 200 | 375 - 392 | 45 - 60 | Medium | Mirror image. Use protective paper. |
Puzzles (Cardboard/Hardboard, Sublimation Coated) | 190 - 200 | 375 - 392 | 60 - 90 | Medium | Mirror image. Pre-press puzzle 5-10s. Cool flat, possibly under weight. |
Stone Slates (Sublimation Coated Photo Rocks) | 195 - 205 | 385 - 400 | 360 - 600 (6-10 min) | Light - Medium | Mirror image. Print face up, slate face down. Long pre-heat of slate can help. EXTREMELY HOT - use gloves. |
Glass Cutting Boards/Photo Panels (Sublimation Coated, White Back) | 200 | 392 | 240 - 360 (4-6 min) | Medium | Mirror image. Print on white coated side. Often pressed image face up, glass face down on print. |
Heat Transfer Vinyl (HTV) |
|
|
|
|
|
Heat Transfer Vinyl (HTV - Smooth/Standard PU) for Fabrics | 150 - 160 | 300 - 320 | 10 - 15 | Medium - Firm | Do NOT mirror image (unless specified by HTV type). Pre-press garment. Peel carrier hot/warm/cold per HTV instructions. |
Glitter HTV for Fabrics | 160 - 170 | 320 - 335 | 15 - 20 | Firm | Do NOT mirror. Pre-press garment. Peel carrier per instructions. |
Transfer Papers |
|
|
|
|
|
Light Fabric Transfer Paper (Inkjet for Cotton/Blends) | 180 - 190 | 355 - 375 | 15 - 30 | Medium - Firm | Mirror image. Pre-press garment. Peel hot/warm per paper instructions. For light/white fabrics. |
Dark Fabric Transfer Paper (Inkjet for Cotton/Blends) | 160 - 175 | 320 - 350 | 15 - 25 | Light - Medium | Do NOT mirror image. Pre-press garment. Weed design, peel from backing, place on garment. Cover with parchment/Teflon. For dark fabrics. |
PU Leather / Faux Leather Blanks (Sublimation-Ready or for HTV) | 180-190 (Sub) / 140-150 (HTV) | 355-375 (Sub) / 285-300 (HTV) | 50-70 (Sub) / 10-15 (HTV) | Light - Medium | Test carefully to avoid melting/scorching. Use protective sheet. For Sub: Mirror image. |
2-Tone Sublimer Blanks (Acrylic/Plastic for Sublimation) | 200 | 392 | 70 (after pre-heat) | Variable (Low-Med) | Do NOT mirror image. Remove back film. Pre-heat clear front 70-100s (element close, no touch). Flip & press. Cool under heavy weight. |
Cap Press Settings
Material / Type | Temperature (°C) | Temperature (°F) | Time (Seconds) | Pressure | Notes / Tips |
---|---|---|---|---|---|
Polyester Caps (for Sublimation) | 185 - 195 | 365 - 385 | 45 - 60 | Medium - Firm | Mirror image. Ensure good contact with curved platen. Use protective paper. |
Cotton/Blend Caps (for HTV application) | 150 - 165 | 300 - 330 | 10 - 20 | Firm | Do NOT mirror image (unless HTV type specifies). Pre-press cap. Peel carrier per HTV instructions. |
Cotton/Blend Caps (for Transfer Paper application) | 160 - 180 | 320 - 355 | 15 - 25 | Medium - Firm | Mirror for light transfers, NOT for dark. Follow paper-specific instructions. |
Mug Press Settings
Material / Coating | Temperature (°C) | Temperature (°F) | Time (Seconds) | Pressure | Notes / Tips |
---|---|---|---|---|---|
Ceramic Mugs (Sublimation Coated, 11oz/15oz) | 190 - 200 | 375 - 392 | 180 - 240 (3-4 min) | Medium - Firm | Mirror image. Tape print tightly. Some pre-heat mug in press. Remove paper immediately. Cool in front of fan or submerge in room temp water. |
Stainless Steel Tumblers/Mugs (Sublimation Coated) | 180 - 195 | 355 - 385 | 60 - 120 (Press) / 240-420 (Oven: 4-7 min @ 180-190°C) | Medium - Firm (Press) | Mirror image. Tape print tightly. If using press, may need to rotate. Shrink wrap + convection oven gives even results. |
Glass Mugs/Tumblers (Sublimation Coated) | 190 - 200 | 375 - 392 | 120 - 180 (Press) / 300-480 (Oven: 5-8 min @ 180-190°C) | Light - Medium (Press) | Mirror image. Be cautious with pressure on glass. Convection oven often preferred for even heating. Results vary significantly. |
Enamel Mugs (Sublimation Coated) | 190 - 200 | 375 - 392 | 120 - 180 | Medium | Mirror image. Tape print tightly. May require specific mug wrap or insert for even pressure. Avoid overheating handle if not coated. |
General Tips for All Heat Pressing:
- Pre-Press: Most garments and some rigid items benefit from a quick 3-5 second pre-press to remove moisture and wrinkles, ensuring better adhesion/transfer.
- Protective Paper: Always use protective paper (e.g., Teflon sheet, parchment paper, plain copy paper, silicone paper) between your heating element and your transfer/substrate, and often between the substrate and the bottom platen to prevent ink bleed-through or scorching.
- Mirror Image: Most sublimation processes require the image to be mirrored before printing. Most standard HTV does NOT require mirroring. Transfer papers vary (light usually mirrored, dark usually not). Always double-check the specific product instructions!
- Even Pressure: Ensure your press is calibrated to apply even pressure across the entire surface. Uneven pressure leads to inconsistent results.
- Calibrate Your Press Temperature: Use a surface temperature probe or heat strips to verify the actual temperature of your heat platen, as built-in display readings can sometimes be inaccurate over time.
- Manufacturer's Instructions: When in doubt, always refer to the specific instructions provided by the manufacturer of your blanks, inks, papers, or vinyl. These are often the most accurate for their particular products.
- Testing is Key: Before running a batch, always test your settings on a scrap piece of the exact material you'll be using. This can save significant time, money, and frustration.
- Environment Matters: High humidity can affect sublimation and transfer papers. Store materials properly and consider a dehumidifier if your workspace is very humid.
This guide was last updated: June 09, 2025. Settings can change, always test.